C95800 (Nickel Aluminum Bronze) Bushings for Fire Pumps
C95800 (Nickel Aluminum Bronze) Bushings for Fire Pumps
High-Performance Self-Lubricating Bronze Bushing Solutions & Technologies. Minimize downtime, extend service life, and reduce costs for dynamic applications.
C95800 (Nickel Aluminum Bronze) Bushings for Fire Pumps
Application-Area Matrix & Material Selection Guide · Materials Coverage Reference, Aluminium Bronze Bushings for Saltwater Pump Applications
Engineered for saltwater service: C95800 nickel-aluminum bronze ranks among the most corrosion-resistant copper alloys on the market. In seawater applications such as pump shafts and impeller bushings, it delivers years of additional service life compared with standard bronzes.
Applications
- Seawater cooling and fire pump shafts
- Desalination plant pump bushings
- Offshore and shipboard pump internals
- Valve stems and guide bushings
C95800 — also known as Nickel Aluminum Bronze (NAB), designated UNS C95800 / EN 1982 CC334G / DIN CuAl10Ni5Fe4 / JIS H5121 CAC703 (AlBC3) / GB ZCuAl10Fe4Ni4 — is a copper-base casting alloy developed for seawater and high-load service. In fire pumps it serves as the primary bearing and friction-pair component where long idle standby, instantaneous reliable start, and dry-start conditions are routine operating states.
1. Application-Area Matrix
Fire pumps are commonly configured as Vertical Turbine (deep-well / seawater lift), Horizontal Split Case, and End Suction types. The C95800 bushing application matrix is summarized below.
| Application Area | Pump Type | Function | Service Condition | Why C95800 |
|---|---|---|---|---|
| Bowl Bushing | Vertical Turbine | Supports the impeller shaft inside the bowl; carries radial rotor load and maintains running clearance between rotating and stationary parts. | Water-lubricated; radial impact from impeller imbalance; possible silt/abrasion. | Dry-start capability with low propensity to seize; erosion and cavitation resistance in flow. |
| Line Shaft Bushing | Vertical Turbine | Provides multi-point radial support to the long drive shaft at each column section; limits shaft deflection and vibration. | Long-term immersion in static (often seawater); sustained rotational friction. | Seawater corrosion resistance and inherent biofouling resistance help prevent seizure during long standby. |
| Stuffing Box / Throttle Bushing | All types | Located at the shaft seal; restricts high-pressure leakage from the casing and supports packing or mechanical seal seats. | High differential pressure; localized turbulence; high-velocity flush. | High hardness and strength resist high-pressure flush erosion and extend seal life. |
| Wear Ring / Casing Bushing | Split Case / End Suction | Fitted at the casing or impeller neck ring; controls recirculation leakage between high- and low-pressure chambers. | Very small running clearance (typically 0.3–0.5 mm); prone to rub contact. | Lubrication compatibility; brief contact with duplex-stainless shaft does not cause galling or lockup. |
| Interstage Bushing | Multistage | Positioned at the diaphragm between adjacent impellers; prevents inter-stage flow bypass. | Inter-stage differential pressure; high-velocity flush. | Resists de-aluminification; maintains dimensional stability in complex hydraulic environments. |
2. Material Selection Rationale
2.1 Composition & Microstructure
Per ASTM B148 (Cast Copper-Base Alloys), C95800 nominal composition:
| Element | Cu | Al | Ni | Fe | Mn | Si (max) | Pb (max) |
|---|---|---|---|---|---|---|---|
| % | 79.0 min | 8.5–9.5 | 4.0–5.0 | 3.5–4.5 | 0.8–1.5 | 0.10 | 0.03 |
Nickel refines the grain structure, stabilizes the microstructure against decomposition to the weak γ₂ phase, and improves both strength and toughness. Iron promotes hard κ-phase precipitates that resist cavitation erosion and abrasion. Together, Ni + Fe provide resistance to de-aluminification (dealuminization) in chloride service.
2.2 Representative Properties
| Property | Value | Note |
|---|---|---|
| Tensile strength (min) | 585 MPa | 85 ksi |
| Yield strength, 0.5% ext. (min) | 240 MPa | 35 ksi |
| Elongation (in 50 mm, min) | 15% | — |
| Brinell hardness | 150–190 HBW | typical range |
| Density | 7.64 g/cm³ | 0.276 lb/in³ |
| Coeff. of thermal expansion | ≈16 µm/m·°C | 20–300 °C |
| Thermal conductivity | 36 W/m·K | — |
| Max. service temperature | ≈400 °C | design ceiling |
2.3 Anti-Galling for Standby-Start Duty
Fire pumps typically run a short weekly or monthly test and remain idle otherwise. At the first seconds of start, the bushing and shaft interface may operate under boundary / dry conditions. If both shaft and bushing were stainless steel, metal-to-metal contact can produce galling and lockup — a critical failure mode for a fire pump.
2.4 Seawater Corrosion & Cavitation Resistance
For offshore platforms, FPSO units, and coastal process plants, the fire-water source is frequently raw seawater. C95800 forms a dense, tenacious aluminum-oxide (Al₂O₃) surface film that delivers pitting and crevice-corrosion resistance superior to conventional tin bronzes (e.g., C93200, C83600) and cast iron. Under fire duty the pump may operate at elevated flow (up to 150% of rated), where cavitation is likely; C95800 provides higher cavitation-erosion resistance than cast stainless steel and conventional tin bronzes.
2.5 Inherent Biofouling Resistance
The copper-rich composition provides inherent resistance to attachment of barnacles, algae, and similar marine growth within the bushing-to-housing clearance. Non-metallic bearings (rubber or plastic) can allow biological blockage during long standby, which may prevent start. C95800 reduces this risk.
3. Cross-Material Comparison
| Alternative | Characteristic / Use | Comparison vs. C95800 (NAB) |
|---|---|---|
| C93200 (SAE 660) High-leaded tin bronze |
Good lubricity; common in fresh-water / general industrial bushings. | C95800 is preferred for seawater service. C93200 has lower strength and is susceptible to erosion-corrosion at high seawater velocities; generally not selected for seawater fire pumps. |
| XM-19 / Duplex Stainless | High strength, high corrosion resistance alloy steel. | Steel-on-steel pairing with the shaft is not advised — galling/lockup risk on start. When the shaft is duplex stainless, the bushing should remain a dissimilar copper-base alloy such as C95800. |
| Polymer / Composite Bearing (thermoplastic or PEEK-type) |
Engineered non-metallic bearing with good wear behavior in continuously running pumps. | Performs well in continuous-duty pumps, but heat dissipation is limited; dry instantaneous start can damage the bearing, and it lacks inherent biofouling resistance. C95800 is the more conservative choice for fire-pump standby duty. |
| C95400 Aluminum bronze |
Standard aluminum bronze; high strength, lower cost than C95800. | C95800 is the more suitable choice for seawater. C95400 contains little or no nickel and is more susceptible to de-aluminification in seawater (loss of properties). C95800 was developed to address this limitation. |
4. Selection Recommendation
4.1 Clearance Design Note
C95800 has a coefficient of thermal expansion (≈16 µm/m·°C) comparable to austenitic stainless steel and somewhat higher than duplex stainless. When setting bushing-to-shaft clearance:
- Apply the applicable minimum allowable running clearance from the project’s pump standard (commonly referenced to API 610 running-clearance tables for offshore-built units).
- Add a small margin for thermal growth so the bushing does not bind at operating temperature.
- Typical wear-ring running clearance is in the 0.3–0.5 mm range for the sizes concerned; the exact allowable value is size-dependent and defined by the governing specification.
4.2 Standards & Specification Caveat
Disclaimer. This document is provided for general technical reference on C95800 (Nickel Aluminum Bronze) bushing application and material selection in fire pumps. Composition, property, and cross-reference data are summarized from published standards (notably ASTM B148) and supplier technical literature; values are typical and may vary by temper, casting method, and specification edition. This guide does not constitute engineering certification or a substitute for a project-specific design review. Selection of materials, dimensions, and clearances must be verified against the current applicable standards (e.g., NFPA 20, API 610), the pump manufacturer’s documentation, and the governing project specification. The publisher accepts no liability for use of this information in procurement or design decisions.
Cross-references: UNS C95800 · ASTM B148 / B505 / B271 · SAE J461/J462 · EN 1982 CC334G · DIN CuAl10Ni5Fe4 · JIS H5121 CAC703 (AlBC3) · GB ZCuAl10Fe4Ni4 · BS 1400 NAB.
Materials
C95800 Aluminium Bronze Bushing
Industries
Pumps, Valves & Hydraulics Bearing Bush, Bushing – Standard & Customized Bearings
Metal Bushing (Lubricated Metal) -Self-Lubricating Bushing Materials
Bushings are specialized, self-lubricating metal components widely utilized across various industries due to their durability and low maintenance requirements. Self-lubricating metal bushings are engineered to function without additional lubrication in numerous applications, thereby minimizing maintenance needs. These bushings are available in various series and configurations, such as flanged bushings and split bearings, to meet specific application requirements.
Metal-Polymer Anti-Friction Plain Bearings
Metal-Polymer Composite Self-lubricating Bushing Material
Steel Back + Porous Bronze Sinter + PTFE