Custom plain bearings
The demand for custom non-standard plain bearings is increasing. We can manufacture copper alloy materials to meet China’s national standards as well as the ASTM (UNS, SAE), EU, and JIS standards.
Bespoke plain bearings
viiplus collaborates with customers to find tailored solutions, offering plain bearings in various materials, sizes, tolerances, and designs.
Timely Delivery
Committed to meeting tight deadlines without compromising on quality, we ensure reliable and efficient production timelines.
Versatility
Capable of handling both small-scale and high-volume orders, we provide seamless support for projects of any size. Additionally, we can develop custom copper alloy materials based on specific customer requirements and drawings.
Cast Bronze · Plain Sliding Bearings · Heavy Port Machinery
Port crane cast bronze bushing: SL on a port crane submittal is a plain sliding bearing abbreviation — sleeve, sliding block, slide bushing or sliding element — as opposed to a rolling-element bearing. CAST BRONZE is the material: usually a tin bronze or an aluminium bronze, frequently with solid-lubricant graphite dispersed through it. The parts are sacrificial wear items in high-friction heavy-lift zones, chiefly the trolley reeving sheave hubs and sheave pins, the boom hinge and A-frame pins, and the trolley and gantry travel drive joints. They are specified where the sliding speed is low, the load reversals repeatedly, the atmosphere is salt-laden, and the position is impractical to reach for greasing. Bearings/Cast Bronze/Port Crane Self-Lubricating Bush:
- Duty class: Oscillating low-speed, reversing
- Dry sliding speed: 0.3–1.0 m/s
- Service temperature:−40~+250 °C, alloy dependent
- Lubrication: Maintenance-free with solid lube
Cast bronze bearing range, graphite-embedded solid bronze bushing flange size
CAST BRONZE SL — Self-Lubricating Bushings for Heavy Port Machinery
Cast bronze sliding blocks, sleeves, or sliding bushings (abbreviated as “SL”) are manufactured or specified for heavy port machinery. These cast bronze self-lubricating bushes are used in quayside container cranes (STS), rubber-tired gantry cranes (RTG), and large bulk material handling equipment, where mechanical assembly submittals and maintenance logs frequently reference high-load components made from cast copper/bronze alloys.
“CAST BRONZE”: The material composition is typically an aluminum bronze or tin-phosphor bronze alloy. These alloys are selected for their high uniform load-bearing capacity, anti-friction properties, self-lubrication, and excellent resistance to harsh, corrosive marine environments.
“SL”: Generally shorthand in heavy machinery drawings for a Sleeve, Sliding Block, or Slide Bushing. These are sacrificial wear parts used in high-friction, heavy-lift zones such as:
-
Trolley travel assemblies or catenary wire rope reeving systems
-
Boom hinge pins and sheave hubs
-
Gantry drive mechanisms and heavy-duty wheel gearboxes
CAST BRONZE SL Graphite — Trolley Reeving
Oilless Bushing Material, Machining Parts
Oilless Bronze Bushing Material Selection & Application Matrix
Explore the complete material selection and application matrix for oilless bronze bushings, comparing CuZn25Al5, CuAl10Ni, and their ASTM/EN equivalents for heavy-duty industrial friction solutions, trolley reeving system bushing.
Cast bronze SL (solid lubricant) graphite bearings are heavy-duty, self-lubricating components used in trolley reeving systems of Ship-to-Shore (STS) and Rubber-Tired Gantry (RTG) cranes. Because trolley reeving sheaves experience continuous high-load, low-speed oscillating motion in harsh, salt-laden port environments, conventional greased bearings frequently fail or leak oil. Heavy Duty Plain Bearings at viiplus.com. Solutions in Principal Markets Worldwide.
Get a Quote for Your Cast Bronze/Port Crane Self-Lubricating Bush!
Send your drawing or sample and receive a manufacturability review, alloy recommendation, and lead time — typically within one business day. Primary Function in Trolley Reeving. In crane reeving assemblies, these graphite-plugged bushings are pressed into the wire rope sheaves or pulley groups.
type of Custom Bearings & Bushings, Flanged Bearings, Custom Oilless Bronze Bushings, Custom Sliding Bearing
Custom Bearings & Bushings Materials & Alloys We Machine,
bronze bushings for sale, cast bronze bushings, Cast Bronze Self-Lubricating Bushes for STS and RTG Port Cranes
Material selection
Alloy map for port machinery sliding joints
Grades are cross-referenced across the Chinese, European and North American systems. Property ranges are typical values and vary with casting method, section size and the governing standard, so they support preliminary selection rather than final design.
| Alloy / grade | Standards cross-reference | Tensile (MPa) | Hardness (HB) | Density (g/cm³) | Behaviour and port machinery use |
|---|---|---|---|---|---|
| CuSn12 | CC483K · GB/T 1176 ZCuSn12 · UNS C92500 family | 280–400 | 80–120 | 8.7–8.8 | Tin bronze with good wear and corrosion resistance and good anti-seizure behaviour. Shock tolerant and forgiving under uneven load. Selected for hook and boom hinge pins, sheave pins, spreader slides, slew ring segments and water-lubricated joints. |
| CuSn10 / CuSn10P | CC483G · GB/T 1176 ZCuSn10 · phosphor bronze family | 250–350 | 90–120 | 8.8 | General purpose bearing tin bronze; the phosphorus addition raises wear resistance and fatigue strength. Common on moderate-load pins and wear plates across reeving and travel assemblies. |
| C93200 / SAE 660 | Leaded bearing bronze · ASTM B306 family | 220–300 | 60–110 | 8.8 | Leaded tin bronze; high conformability and anti-friction performance, tolerant of out-of-alignment mounting and intermittent lubrication. Suitable where a joint is still reachable for greasing. |
| CuAl10Ni5Fe4 | CC333G · GB/T 1176 ZCuAl10Ni5Fe4 · UNS C95500 | 600–750 | 170–210 | 7.6–7.8 | Nickel aluminium bronze. High load capacity combined with seawater resistance; the reference selection for boom hinges, catenary tensioners, marine pivots and immersed service. Requires sharp tooling and rigid setup in machining. |
| CuAl10Fe3 | CC305G family · UNS C95400 | 517–621 | 150–170 | 7.45 | Aluminium bronze with high wear resistance and good machinability. Widely used for trolley and gantry travel wheel hubs and sheave hubs where the environment is marine but immersion is not expected. |
| CuAl10Fe3Mn2 | BA1032 family | 500–550 | 110–120 | 7.6 | Aluminium iron manganese bronze; hard, abrasion resistant, tolerant of shock and elevated temperature. Applied to travel wheel hubs, trolley rail rollers and grab bucket hinge pins in abrasive service. |
| SAE 841 | Oil-impregnated powder bronze · ASTM B438 family | ≈97 | 45–55 HRB | 6.4–6.8 | Sintered and vacuum oil-impregnated, 18–22 % porosity, oil content 24–27 % by volume. Suitable for small to medium pins at moderate load and limited temperature. Not the reference choice for main load joints. |
| SAE 863 | Higher-density powder bronze · ASTM B438 family | ≈145 | higher | 7.2–7.6 | Higher density and lower porosity than SAE 841, giving higher load capacity at the cost of self-lubricating reserve. Available as solid and cored bar for machined-to-print parts. |
SAE 841 and SAE 863 sintered grades are normally supplied in a fixed size range and are not intended for high-load, low-speed heavy-lift joints. For those positions, specify a cast or forged grade machined to the drawing. Grade equivalences must be confirmed against the governing standard before ordering.
Reading the submittal: what CAST BRONZE and SL actually instruct
Purchase orders and mechanical assembly submittals abbreviate heavily. Two tokens carry most of the design intent, and they describe different things — one is the component form, the other is the material and its lubrication state.
| Token on drawing / BOM | What it designates | Why it matters for the buyer |
|---|---|---|
| SL | A plain sliding bearing element. Expanded on crane and fabrication drawings as sleeve, sliding block, slide bushing or sliding bearing. | Confirms the item is a sacrificial wear part, not a load-carrying structural member and not a rolling-element bearing. Dimensions come from the sleeve bore and outside diameter, or from the block face and thickness. |
| SL + (solid lubricant) | The same component form supplied with a solid lubricant dispersed in the bronze matrix — graphite plugs or a graphite-loaded surface. | Removes the greasing step from the maintenance schedule. This is the condition normally intended where access is restricted or the environment is corrosive. |
| CAST BRONZE | The material family. Usually an aluminium bronze or a tin phosphor bronze; a phosphor bronze designation indicates the phosphorus level. | Alloy choice sets the load capacity, the wear behaviour under shock, and the seawater resistance. The material family alone does not identify a grade — a cross-reference to a standard is normally required. |
| BRG / BLK / THR / WDW | Adjacent abbreviations distinguishing bearing, block, thrust and wear-plate items within the same assembly. | A thrust or wear-plate item in the same package is usually a sliding pad rather than a cylindrical bush, and is supplied in plate or bar form. |
Abbreviations are manufacturer-specific. The expansion of SL is confirmed from the submittal legend, the bill of material and the corresponding line in the maintenance log — not assumed.
Application map
Where cast bronze SL bushes sit on STS, RTG and bulk handling equipment
The positions below are grouped by crane system. Within each group the exact position depends on the crane type, whether the trolley is rope-towed or semi-rope, and the number of rope falls in the reeving layout.
| Zone | Component and SL form | Duty and load direction | Alloy typically considered |
|---|---|---|---|
| Trolley reeving | Trolley reeving sheave hub bush — flanged bronze sleeve pressed into the sheave bore | Continuous rope tension while the trolley is stationary, reversed each hoist cycle; oscillating rotation on the pin | CuAl10Ni5Fe4, CuAl10Fe3 high load |
| Trolley reeving sheave pin bush — sleeve on the fixed pin or tube | Same oscillating rotation, load carried in bending on the pin | CuAl10Ni5Fe4, CuAl10Fe3, CuSn12 where impact dominates | |
| Sheave thrust washer / flanged thrust bush at the sheave hub | Axial load from rope tension angle; steady during a lift | CuSn12, CuAl10Fe3 axial | |
| Catenary and rope tensioning sheave bushes at the backreach tensioner | Sustained static preload for the duration of the lift | CuAl10Ni5Fe4, CuAl10Fe3 sustained preload | |
| Anti-derailment slide blocks and trolley frame wear strips | Linear sliding along the trolley frame, rope-contact guiding | Bronze with solid lubricant, wear plate grade | |
| Hoist and rope handling | Hoist sheave and headblock sheave hub / pin bushes | High rope tension, continuous rotation, frequent stopping and starting | CuAl10Ni5Fe4, CuAl10Fe3 abrasive wear |
| Spreader and twistlock slide blocks, headblock guide slides | Linear sliding under load, contamination from cargo and dust | Bronze with solid lubricant; tin bronze where impact peaks occur | |
| Hook block sheave hub and hook shank bush | Block rotation, shock loading on snagging | CuSn12 shock tolerant | |
| Boom and structure | Boom hinge and luffing pivot pins (boom raising hinge) | Carries the boom and outreach load; heavy static with reversal on hoist | CuAl10Ni5Fe4, CuAl10Fe3 heavy load |
| A-frame and backstay tie-rod bushes | Static tension, minimal rotation, difficult access | CuAl10Ni5Fe4 inaccessible | |
| Boom rest sliding blocks and girder tie-rod pins | Linear sliding when the boom is landed for ship movement | Bronze with solid lubricant, wear plate grade | |
| Travel and drive | Trolley travel wheel hub bushes (trolley running on boom rails) | Rolling contact, flange loading from crane skew and rail joints | CuAl10Fe3, CuAl10Fe3Mn2 shock + wear |
| Gantry travel wheel hub bushes on rail-mounted cranes; steering kingpin and kingpin bushes on RTG | Long travel duty, severe shock at rail joints, steering articulation cycles | CuAl10Fe3Mn2, CuAl10Ni5Fe4 severe duty | |
| Travel gearbox output bushes, coupling bushes, rail clamp and storm brake pivot bushes | Static housing loads, pivoting motion, gearbox oil mist environment | CuSn12, CuAl10Fe3 | |
| Bulk material handling | Slew ring and luffing ring wear pad segments (ship unloaders, level-luffing cranes) | Very large area, slow rotation, seawater exposure, abrasive cargo contact | CuAl10Ni5Fe4, CuSn12 seawater |
| Grab and bucket hinge pins, side cutter pins | Shock loading on dig, abrasive slurry environment | CuSn12, CuSn10 impact + slurry | |
| Chute liners, feeder pan wear shoes, conveyor skirt wear plates | Linear sliding of bulk material; highly abrasive | High-tin bronze wear plate, aluminium bronze per wear rate |
Rows are indicative duty positions, not a specification. Any single position must be confirmed against the crane builder’s parts submittal for the machine in question.
How a solid-lubricated bronze bush performs in a reeving sheave
In a trolley reeving system the hoist rope runs over sheaves that carry the full rope tension while the trolley is stationary, and the sheave pin reverses direction of load at every hoist stroke. This is a boundary-lubricated oscillating duty, not a hydrodynamic one, which is why the lubrication method matters more here than the nominal load.
Indicative section through a trolley reeving sheave. The bronze bush is the sacrificial interface: the pin is the counterface, the solid lubricant is the film former, and the sheave bore is the housing. Geometry shown is illustrative and not a machining drawing.
The duty does not build a fluid film
Trolley reeving sheaves and hinge pins run at low sliding speed with frequent load reversal. The speed is too low for a hydrodynamic film to establish, so the joint works in the mixed and boundary regime where the contacting asperities carry the load. This is the regime in which the material pair and the lubricant actually present at the interface decide the wear rate.
Salt-laden atmosphere works against grease
Coastal terminals operate in a chloride-laden atmosphere with condensation cycling. Grease at a joint is progressively contaminated with salt and abrasive particles, and its film strength at the rolling and sliding contact drops. Aluminium bronze develops a stable surface oxide film that resists this attack; nickel aluminium bronze is the reference choice where seawater immersion or continuous wetting applies.
Access decides whether lubrication actually happens
Trolley reeving components sit above the boom, above water, or inside a machinery house reached only by access platforms. Greasing these positions requires rope access or an overhead jib. Where the interval is short and access is awkward, the lubrication step is deferred shift after shift and the first indication of failure is often a seized pin or a rope jump rather than a scheduled wear-out.
Contamination handling
Bronze grades with good embeddability absorb fine particles that bypass the seals instead of letting them cut the counterface. Where the counterface is the pin rather than the shaft, and the pin is the cheaper or the harder-to-replace item, this is a decisive argument — the wear is distributed into the part designed to be replaced.
Indicative material comparison for the same joint
Comparison is between lubrication strategies for an equivalent high-load, low-speed, marine-atmosphere joint. Values describe behaviour, not a guarantee; the governing limits are set by the governing standard and by the crane builder’s submittal.
| Attribute | Cast bronze with solid lubricant | Cast bronze, greased | Hardened steel, greased | Polymer / composite | Rolling-element bearing |
|---|---|---|---|---|---|
| Lubrication source | Graphite in the matrix; no external supply required | Grease fitting and routine greasing | Grease fitting and routine greasing | Self-lubricating polymer | Oil bath or grease |
| Behaviour at low speed with reversing load | Designed for boundary and oscillating duty | Depends entirely on grease presence and grade | Metal-to-metal contact when grease film is lost | Good, but load capacity limited | Poor fit — needs rolling speed |
| Load capacity at this duty | High | High | High | Low to fair | High, but not suited to oscillating pivots |
| Salt spray and seawater exposure | Corrosion resistant; NAB grades suited to immersion | Corrosion resistant; joint depends on the grease | Corrosion and seizure risk at exposed pins | Corrosion resistant | Requires sealing and regular lubrication |
| Abrasive contamination | Good embeddability in suitable tin bronzes | Particles held in the grease film | Particles cut the contact | Particles can embed and glaze the surface | Requires filtration and sealing |
| Failure mode | Gradual, measurable wear; part is a designed sacrificial item | Progressive wear, then seizure if the interval is missed | Scuffing and seizure, rapid once lubrication is lost | Deformation, cracking, thermal softening | Point and roller damage, spalling |
| Maintenance requirement | Inspection and replacement on measured wear | Greasing rounds plus inspection | Greasing rounds plus inspection | Inspection and replacement | Lubrication and condition monitoring |
| Availability of the joint for service | Unaffected — no access required to lubricate | Access platform, rope access or overhead jib | Access platform, rope access or overhead jib | Unaffected | Access required for greasing |
Bronze grades with a lead addition carry improved anti-friction and conformability but are not permitted in some food, drinking water and hygiene applications. Confirm the alloy before use where those constraints apply.
Engineering data
Preliminary selection limits and fitting requirements
The following values support a preliminary selection or a quotation enquiry. They are indicative engineering ranges compiled from published bearing practice, not guaranteed design allowables. Final limits are set by the governing standard, the casting method and the duty data for the machine.
Preliminary selection limits by lubrication mode
| Lubrication mode and material | Continuous P·v N/mm² · m/s |
Static pressure N/mm² |
Sliding speed m/s |
Service temperature °C |
Friction coefficient indicative |
|---|---|---|---|---|---|
| Sintered oil-impregnated bronze (SAE 841 / 863) | ≤ 1.75 | ≤ 35 | up to ~6 | −12 to +105 | 0.02–0.06 |
| Cast bronze with graphite plugs, dry | ≤ 1.0 | 60–120 | 0.3–1.0 | −40 to +250 | 0.12–0.25 |
| Cast aluminium bronze with graphite plugs, dry | ≤ 1.0 | 80–120 | 0.3–1.0 | −40 to +300 | 0.12–0.25 |
| Cast aluminium bronze, externally greased | 4–6 | up to 150 | up to 2.5 | −40 to +120 | 0.05–0.15 |
A dry graphite-plugged bushing trades sliding limit for load capacity: raising the graphite volume fraction increases the permissible P·v and lowers the permissible static pressure. Where an external lubricant is available and reliable, a greased aluminium bronze joint carries a substantially higher P·v.
Counterface, housing and fitting requirements
| Item | Requirement | Note |
|---|---|---|
| Shaft or pin hardness | ≥ 45 HRC for moderate-duty tin bronze; ≥ 54 HRC for aluminium bronze or high-load pivots | Below these levels the counterface wears as fast as the bush |
| Shaft surface finish | Ra 0.4–0.8 µm | Rougher surfaces rupture the film at local contact points |
| Housing bore | H7 | Housing bore condition governs whether the bush can be pressed without distorting the bore |
| Bush outside diameter | r6 or u6 | Sets a light, predictable press fit |
| Interference | 0.0005–0.0015 mm per mm of diameter | An incorrect press fit is a common cause of early bush failure |
| Diametral clearance | 0.001–0.002 mm per mm of shaft diameter | Add clearance where the joint sees significant temperature excursion |
| Post-installation verification | Re-measure the bore after pressing | The bore contracts by a large proportion of the interference; a part that measured correctly before pressing may not after |
| Alignment | Correct within the housing design; avoid edge loading | Edge loading produces circumferential wear at one side of the bore rather than even wear |
| Installation tooling | Press on the bush, never on the pin | Prevents galling of the bore and distortion of the part |
| Break-in | Initial operation at reduced load before full duty | Allows the bearing to seat and the lubricant film to establish |
Environment classification, where specified by the terminal operator, is commonly referenced to ISO 9223 for the corrosivity of atmospheres and to the protective paint systems of ISO 12944. Where the part is installed in a classed vessel structure, class-society material approval may need to be requested separately.
Solid lubricant
Graphite volume fraction and plug pattern
Both the fraction and the pattern are design variables. Specifying them explicitly on the drawing is what makes a replacement part repeatable; a part described only as self-lubricating bronze is not a reproducible specification.
| Motion type on the joint | Typical plug pattern | Reason for the pattern |
|---|---|---|
| Oscillating rotation — trolley reeving sheave hub, boom hinge | Segmented, or a helical arrangement along the bore | Distributes lubricant along the arc swept by the pin so a film is maintained through the reversal rather than only at one angular position |
| Continuous rotation — travel wheel hub, rotating sheave | Axial rows, evenly distributed | Carries lubricant around the full circumference and maintains a uniform annular film |
| Linear sliding — wear pads, slide blocks, chute liners | Directional stripes or a uniform open-pore grade | Lubricant is drawn along the direction of travel rather than being displaced out of the contact zone |
Record the specified volume fraction and pattern on the drawing or parts submittal, on the part marking where practical, and in the maintenance record, so that repeat replacements are matched to the original design.
Maintenance
Inspection, wear limits and replacement triggers
A bronze plain bearing is a wear item with a measurable life. Measuring it converts an unplanned failure into a scheduled replacement.
How to measure clearance
- Split housings: with the machine stopped and the upper half removed, insert feeler gauges between the pin and the bush bore on the unloaded side; the reading equals the diametral clearance.
- Closed housings: apply a known upward force to the pin and measure vertical displacement with a dial indicator; the displacement equals the diametral clearance.
- In service: measure remaining wall thickness with an ultrasonic thickness gauge through the housing wall and calculate clearance from the original dimensions.
- Trend rather than inspect once: record the measured clearance at each intervention so the wear rate for that specific joint is known rather than assumed.
Replacement criteria
| Measured condition | Action |
|---|---|
| Clearance at 200 % of design clearance | Replace at the next planned shutdown; do not defer |
| Clearance above 300 % of design clearance | Remove from service — risk of pin-to-housing contact |
| Diametral clearance above roughly 1.5–2 % of pin diameter | Replace. This is the commonly applied heavy-industry rule |
| Bore increase beyond roughly 0.075–0.150 mm over specification | Replace |
| Scoring, seizure marks or discolouration on the bore | Replace immediately regardless of the clearance reading |
| Wall thickness below about 80 % of nominal | Replace |
| Consistent rise in operating temperature at the joint | Investigate and replace; a thermal shift often precedes measurable wear |
Interval figures quoted in maintenance literature vary widely because wear rate is a function of load, duty cycle, lubrication and environment. The crane builder’s stated limits and the machine’s own inspection records take precedence over any generic interval.
Failure mode and root cause
| Observed condition | Likely cause | Action beyond replacing the bush |
|---|---|---|
| Circumferential wear at one side of the bore | Misalignment or edge loading | Check bore geometry, housing alignment and pin runout |
| Uniform wear over the full length | Normal progressive wear | Confirm the wear rate is consistent with the duty; if not, re-check the load data |
| Grooves and scoring in the bearing surface | Abrasive particles bypassing the seal | Improve exclusion; consider a grade with higher embeddability |
| Pitted or thinned bearing surface | Corrosion, often combined with wet cycling | Move to a nickel aluminium bronze and review the sealing |
| Seizure, smeared surface, high temperature | Lubrication was not present at the interface | Review the lubricant specification and the interval; check the solid lubricant fraction specified |
| Premature wear after installation | Loss of clearance through pressing, or an incorrect press fit | Re-measure the bore after installation and record it |
Enquiry data
What to send for a quotation
A drawing gives the fastest route. Where the part is no longer drawn, a worn sample plus a few key dimensions is usually sufficient for an initial quotation.
- Pin or shaft diameter, material and hardness
- Bush outside diameter and length
- Housing bore diameter and housing material
- Load magnitude and direction
- Duty cycle and operating hours per day
- Sliding speed or oscillation frequency
- Working temperature at the joint
- Environment: salt spray exposure class, immersion, dust or slurry
- Required fits, clearances and surface finish
- Solid lubricant fraction and pattern, if specified
- Drawing, or a worn part plus key dimensions
- Quantity and required delivery date
Technical FAQ
Questions frequently raised at enquiry stage
What does SL mean on a port crane bronze part drawing?
On heavy machinery drawings and mechanical assembly submittals, SL is a drawing abbreviation for a plain sliding bearing rather than a rolling-element bearing. Depending on the OEM or the fabrication package it is expanded as sleeve, sliding block, slide bushing, sliding bearing, or solid-lubricated item. The expansion is manufacturer-specific, so the parts submittal, the bill of material legend and the maintenance log entry must be read together to confirm which form the item takes. The same abbreviation is also used for the material condition, for example solid lubricant filled, which is a separate attribute from the component shape.
Which parts of an STS or RTG crane are cast bronze SL bushes used in?
The main duty zones are trolley reeving sheave hubs and sheave pins, catenary and rope tensioning sheaves, hoist sheave and headblock hubs, boom hinge and A-frame pins, trolley and gantry travel wheel hubs, travel gearbox output bushes, spreader and twistlock slides, and on bulk handling equipment the slew ring wear pad segments, grab bucket hinge pins and chute wear shoes. Within each zone the specific positions differ by crane type, trolley arrangement and rope reeving layout.
Why are greased plain bearings replaced with self-lubricating bronze in port machinery?
Three conditions drive the change. First, reeving sheaves and hinge pins run an oscillating duty at low sliding speed with frequent load reversal, so a hydrodynamic oil film does not form and the joint works in the boundary regime. Second, salt-laden marine atmosphere and condensation attack steel pins and wash grease out of the joint. Third, many of these positions are above the boom, inside the machinery house or over water, so the greasing interval is repeatedly skipped in practice. A cast bronze bush with solid-lubricant graphite removes the greasing step and does not depend on a fluid film for its primary lubrication.
How do I select the alloy for a trolley reeving bush?
For oscillating rotating duties on a sheave hub or pin, aluminium bronze such as CuAl10Ni5Fe4 or CuAl10Fe3 gives the load capacity and wear resistance needed at low speed under rope tension. Where impact and shock peaks dominate over static load, a tin bronze such as CuSn12 is more forgiving because it deforms rather than cracks. Where the joint is greased reliably and speed is higher, a leaded tin bronze bearing grade remains economical. Continuous water lubrication or seawater immersion points to a nickel aluminium bronze. Sintered SAE 841 and SAE 863 grades are suitable for smaller, cooler, moderate-load pins rather than main load joints.
What shaft and housing requirements apply to a cast bronze SL bush?
Specify a housing bore to H7 and a bush outside diameter to r6 or u6 to obtain a light press fit, typically 0.0005 to 0.0015 mm interference per mm of diameter. The shaft or pin surface is normally required at about 45 HRC for moderate-duty tin bronze and about 54 HRC for aluminium bronze or high-load pivots, with a surface finish in the region of Ra 0.4 to 0.8 µm. Running clearance is usually set at 0.001 to 0.002 mm per mm of shaft diameter. The bore must be re-measured after pressing, because the bush contracts by a large part of the interference.
How is a worn bronze bushing measured and when is it replaced?
Measurement is by bore micrometer on the installed or removed bush, by dial indicator on pin displacement, or by ultrasonic thickness gauge through the housing wall where the part is in service. Replacement is normally triggered when diametral clearance reaches about 1.5 to 2 percent of the pin diameter, or when clearance reaches twice the design value and the part is changed at the next planned shutdown, or when clearance exceeds three times design and the unit is stopped. Scoring, seizure marks or a loss of wall thickness beyond about 20 percent of nominal call for immediate replacement regardless of clearance.
How much graphite should a self-lubricating bronze bush contain?
The solid lubricant volume fraction, commonly in the range of about 10 to 25 percent by volume, and the plug pattern are both design variables rather than fixed numbers. A larger graphite fraction raises the dry sliding limit and lowers the load capacity; a smaller fraction raises the load capacity and reduces the film completeness. The pattern also follows the motion: segmented or helical patterns for oscillating rotation, axial rows for continuous rotation, and directional stripes for linear sliding. Record the specified fraction and pattern on the part, in the submittal and in the maintenance record so replacements are matched.
What data is needed to quote a replacement cast bronze SL bush to print?
Send the pin or shaft diameter and material, bush outside diameter and length, housing bore and material, load magnitude and direction, duty cycle, sliding speed, working temperature, environment such as salt spray exposure class, required fits and clearances, quantity and required delivery date. A drawing is preferred; for reverse engineering a worn part plus a few key dimensions and photographs of the assembly is usually enough for an initial quotation.
Cast bronze bearing range, Graphite-embedded solid bronze bushing
Send the submittal or the worn part: Cast bronze sleeves, flanged bushes, sliding blocks, thrust washers and graphite-plugged wear parts, machined to drawing or reverse-engineered from a sample. Provide the drawing or the key dimensions and the duty conditions, and the alloy and solid lubricant specification can be confirmed against your operating data before quotation.
viiplus@viiplus.com. Figures in this page are indicative values for preliminary selection and are not guaranteed design allowables. They depend on casting method, section size, solid lubricant fraction and operating duty. Final selection must be verified against the governing standard, the crane builder’s submittal and the machine’s own inspection data.
Scope and limitations. This page is a general engineering reference on cast bronze plain sliding bearings for heavy port machinery. It does not constitute a design, a calculation, or a suitability statement for any specific crane, joint or application. Material property values are typical ranges and vary with casting method, section size, heat treatment and the standard applied. Allowance limits depend on the solid lubricant fraction, the fit, the counterface condition and the actual duty. Component positions listed are indicative duty zones and must be confirmed against the parts submittal for the machine concerned. Replacement intervals quoted are generic and are superseded by the crane builder’s stated limits and the operator’s own inspection records.